Abstract: |
||||
|
In this paper an effort is made to find the stress concentration factor (Kt) near the crack tip in a plate having different crack length to width ratio by applying the compressive load on the rectangular plate with an edge crack. Firstly the material fringe value is determined or calculated by loading the circular disc on polariscope under compression. The stress concentration in the rectangular plate with an edge crack is calculated & at the end of this paper a graph is plotted between stress concentration factor and the crack length to width ratio of the rectangular plate. |
||||